Skip to content

Manufacturing & Distribution

Coated coil fins for coastal sites

  • Manufacturing & Distribution
  • 1 min read

Near the sea, aluminium fins lose their grip on the copper tubes long before they fall off, and the coil loses capacity with them.

The mechanism is galvanic. Copper and aluminium in contact, wetted by condensate that has picked up chloride from sea air or sulphur compounds from industrial exhaust, form a cell, and the aluminium is the metal that gives way. The fin-to-tube bond goes first. Once a fin no longer touches the tube it stops carrying heat, even while it still looks attached.

A coating keeps the water away from the joint, and the two usual routes differ a lot. Pre-coated fin stock is coated before the fins are stamped, so every cut edge is bare metal and the coating on the tube collars is cracked by forming and expansion. A coating applied after the coil is built, e-coat or a sprayed epoxy or polyurethane, reaches the edges and joints, and costs more.

Coating costs some heat transfer, because it adds a thin layer of resistance on the fin. Manufacturers publish a correction factor for it, and the coil selection should use that factor rather than the bare-coil rating. In exchange, the coil keeps its capacity longer on a coastal or industrial site.

For an AeroSano AHU going to such a site, write the coating process into the datasheet and ask for the salt-spray test report and the capacity correction with the offer.

Is anyone in your plant looking at the fresh-air coil fins, or only at the filters in front of them?

Related

More on this subject